In the operation of CANDU reactors, the Zr-2.5Nb pressure tubes holding the cooling water and fuel bundles are susceptible to hydride cracking-induced crack initiation mechanisms, known as delayed hydride cracking and overload crack initiation. For structural integrity evaluation of CANDU pressure tubes, of fracture toughness and hydride crack initiation models were developed. However, the hydride […]